FS25
It is used in steel making and foundry industry for deoxidization and as an alloying element in the production of corrosion-and heat-resistant, electrical and spring-spring steels.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | ferrosilicium |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 1415-93 | 23–29 | < 1 | < 0.8 | < 1 | < 0.06 | < 0.8 | < 0.02 |
Information on suppliers
Analogues
| USA |
|---|
| A 100 Grade F |
Standards
| Standard | Description |
|---|---|
| GOST 1415-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |