FS40L15
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ca, % | Al, % | La, % |
|---|---|---|---|---|---|---|
| TU 14-141-99-90 | 2–53.8 | 8.2–81.8 | 0.2–3 | 1–7 | < 8 | 15–20 |