FS60Ba22
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ba, % | Al, % | P, % |
|---|---|---|---|---|---|---|---|
| TU 14-5-160-84 | 3.16–22 | 46.16–73.84 | < 0.4 | < 0.4 | 20–25 | 3–6 | < 0.04 |