FSCr45
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Cu, % | Zr, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-5-83-87 | 12.4–35 | 20–30 | < 3 | 22.4–67.6 | < 9 | < 0.2 | < 0.2 | < 0.2 |
Note: As agreed: Cu <0.5%; Al <4%
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-5-83-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Cu | % | Copper |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |