FVd12S12
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | V, % | Al, % | P, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-141-08-91 | 38.5–85 | 5–20 | < 10 | < 3 | < 5 | 10–15 | < 8 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-141-08-91 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |