GFI1
Iodide hafnium produced brand GFI1 in accordance with the requirements of GOST 22517−77
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hafnium iodide |
Chemical composition
| Standard | Hf, % |
|---|---|
| GOST 22517-77 | 99.5 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Hf | % | Hafnium |