Ch-0
It is used as a feedstock for producing high purity gallium and other purposes
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Metals and alloys |
Gallium |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
Ga, % |
| GOST 12797-77 |
< 0.0003 |
< 0.0005 |
< 0.0003 |
< 0.002 |
< 0.0001 |
< 0.0001 |
< 0.0003 |
< 0.0006 |
< 99.99 |
Information on suppliers
Casting and technological parameters
| melting point, °C |
Boiling temperature, °C |
| 29.8 |
2203 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| Ga |
% |
Gallium |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Boiling temperature |
°C |
The boiling point, boiling point is the temperature at which the liquid under constant pressure boils. |