GOST 31570-2012
Workpieces from alloys based on Nickel for prosthetic dentistry.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Cr, % | Ni, % | Mo, % |
|---|---|---|---|
| GOST 31570-12 | > 20 | 76 | > 4 |
Note: The chemical composition must provide mechanical properties. Chemical framework composition. The chemical composition is determined by agreement.
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 31570-12 | GOST 31570-12 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cr | % | Chrome |
| Ni | % | Nickel |
| Mo | % | Molybdenum |