GOST R 51767-01
Workpieces from alloys based on Nickel for prosthetic dentistry.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Cr, % | Ni, % | Mo, % |
|---|---|---|---|
| GOST Р 51767-01 | > 20 | 76 | > 4 |
Note: A different proportion of the main alloying elements is allowed provided that the remaining requirements of the standard are met
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST Р 51767-01 | GOST R 51767-01 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cr | % | Chrome |
| Ni | % | Nickel |
| Mo | % | Molybdenum |