ZHS3LS
Production of ingots and cast rods intended for further refining in the production of shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90127 - 85 | < 2 | < 0.6 | < 0.015 | < 0.6 | 4–5 | 15–18 | 2.4–3 | 58.605–70.15 | < 0.015 | 2.4–3 | < 0.015 | < 0.015 | 0.05–0.12 | < 0.015 | 3–4.5 | 3–4.5 |
Information on suppliers
Long-term strength
| Standard | Treatment | Температура испытаний, ° С | Постоянно приложенное напряжение, МПа | Время до разрушения в часах, ч |
|---|---|---|---|---|
| OST 1-90127 - 85 | Heating to a temperature of 1190 ± 30 ° С, holding 3.5–4.5 hours, air cooling | 950 | 120 | 100 |
Standards
| Standard | Description |
|---|---|
| OST 1-90127 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |