H13YU4
resistance to the elements; heat-resisting alloy in an oxidizing atmosphere,
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With high electrical resistance |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | < 1 | < 0.7 | 12–15 | < 0.3 | < 0.6 | 3.5–5.5 | < 0.035 | < 0.15 | < 0.025 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |