X25N13ATL
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
N, % |
| OST 108.961.04-80 |
57.87–63.69 |
< 0.7 |
1–1.5 |
23–25 |
0.1–0.2 |
< 0.3 |
12–14 |
< 0.025 |
0.13–0.2 |
< 0.025 |
0.08–0.18 |