X70A (XA1)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Cr, % | Zn, % | Al, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| TU 14-5-184-87 | < 1 | < 1 | 67.8–84.95 | > 0.05 | 15–30 | < 0.1 | < 0.05 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-5-184-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Cr | % | Chrome |
| Zn | % | Zinc |
| Al | % | Aluminium |
| C | % | Carbon |
| S | % | Sulfur |