H99
In the steel and foundry industry for alloying of special steels and alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Chromium metal |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Bi, % | Cr, % | Cu, % | Zn, % | Sb, % | Al, % | Pb, % | As, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5905-2004 | < 0.5 | < 0.2 | < 0.004 | < 0.0005 | > 99 | < 0.02 | < 0.01 | < 0.008 | < 0.5 | < 0.001 | < 0.01 | < 0.02 | < 0.03 | < 0.02 |