XH32TY (EP985)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Ni, % | Sb, % | V, % | Al, % | Pb, % | As, % | P, % | C, % | S, % | O, % | Mo, % | N, % | W, % | H, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 1333-159-00220302-2011 | 39.253–50.6875 | 0.0005–0.65 | 0.0005–0.74 | 19–23 | 0.25–0.8 | < 0.2 | < 0.01 | 30–34 | < 0.01 | 0.0005–0.1 | 0.0005–0.45 | < 0.01 | < 0.01 | < 0.03 | 0.06–0.1 | < 0.02 | < 0.005 | < 0.5 | < 0.006 | 0.0005–0.1 | < 0.006 |
Note: Pb + Sn + As + Zn <0.15
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| BGH 4959 | JS Alloy 800 H |
Standards
| Standard | Description |
|---|---|
| TU 1333-159-00220302-2011 | |
| TU 14-1-2762-80 | |
| TU 14-1-2912-80 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| V | % | Vanadium |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| O | % | Oxygen |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
| W | % | Tungsten |
| H | % | Hydrogen |