Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ST CKBA 010-2004 | 36.98–47.1 | < 0.6 | 1–2 | < 0.5 | 14–16 | 1.1–1.5 | < 0.25 | 34–38 | < 0.1 | < 0.1 | < 0.03 | < 0.12 | < 0.02 | < 0.1 | < 0.2 | 2.8–3.5 |
Note: By agreement of the parties, a higher proportion of Mo is allowed, subject to a corresponding decrease in W at the rate of replacing it with Mo in a 2: 1 ratio
Note: OST 108.958.04-85: as agreed: S + P <0.035
Information on suppliers
Standards
| Standard | Description |
|---|---|
| ST CKBA 010-2004 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |