HN35VTR (EI725)
a sheet for housing and guide vanes of turbines, operating at temperatures up to 750−800 degrees.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Heat resistant steels and alloys |
Heat resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
W, % |
Se, % |
|
37.725–45.9 |
< 0.6 |
< 1 |
14–16 |
1.1–1.5 |
35–38 |
< 0.03 |
< 0.1 |
< 0.02 |
4–5 |
< 0.025 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
206 |
|
13 |
8280 |
| 100 |
|
14.1 |
13.4 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Sheet |
|
|
|
|
750–800 |
400–450 |
21 |
900 |
Hardening of 1130-1150 ° C, 2 h, the air aging of 750 ° C, 24 h, air |
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy |
|
|
217 |
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| W |
% |
Tungsten |
| Se |
% |
Selenium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |