ХН50МБВЮ
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | Al, % | C, % | Nb, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|
| 8 | 15 | 58.2–58.4 | 1 | < 0.2 | 5.3 | 7.5 | 4.8 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |