KhN54MVTN-VI (ChS94-VI)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Bi, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | Al, % | Pb, % | P, % | C, % | S, % | Mo, % | N, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 2–3.5 | 1–2 | 0.065 | < 5.0E-5 | < 0.3 | 12.8–14.4 | 2–3 | < 0.1 | 50.43745–60.125 | < 0.0005 | 1.5–3 | < 0.001 | < 0.008 | 0.11–0.17 | < 0.008 | 12.2–13.2 | < 0.01 | 8.2–9.8 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
| W | % | Tungsten |