XH60KVMYUTBL (TsNK21P)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
B, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
C, % |
Nb, % |
Mo, % |
W, % |
| TU 1-801-288-91.Р2 |
0.008–0.015 |
< 0.3 |
10–11.5 |
20–22 |
3–3.8 |
54.865–61.342 |
2.1–2.7 |
< 0.02 |
0.05–0.1 |
0.5–0.9 |
1–1.2 |
2–2.6 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| C |
% |
Carbon |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |