XH60KVMYUTL (TsNK7P)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
B, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
C, % |
Mo, % |
W, % |
| TU 1-801-288-91.Р2 |
0.008–0.015 |
< 0.3 |
8–9.5 |
14–15.5 |
3.6–4.4 |
57.955–64.322 |
3.6–4.3 |
0.07–0.13 |
0.2–0.7 |
6.2–7.2 |