HN60MB (EP758U)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.5 | < 0.1 | < 0.5 | 23–25 | 0.01–0.16 | 54.465–60.89 | < 0.025 | < 0.03 | < 0.02 | 0.1–0.2 | 16–19 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |