HN68KMBTYU-ID (EK-104-ID)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-1213-75 |
< 2 |
< 0.5 |
< 0.4 |
4.5–5.5 |
16.5–18 |
0.8–1.2 |
60.99–69.6 |
0.4–0.8 |
1–1.4 |
< 0.015 |
< 0.08 |
< 0.015 |
5.7–6.6 |
1.5–2.5 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |