XH70KVMYUTL (TsNK17P)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
B, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
C, % |
Nb, % |
Mo, % |
W, % |
| TU 1-801-288-91.Р2 |
0.5–2 |
0.01–0.015 |
1–1.7 |
12.8–14 |
5–5.6 |
66.11–72.59 |
4–4.6 |
< 0.025 |
0.1–0.15 |
0.3–0.7 |
0.7–1.4 |
3–3.7 |