XH70VMTKB (ChS70)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Co, % | Cr, % | Ti, % | Ni, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|
| 8.4 | 9 | 8 | 3.6 | 69 | 0.2 | 1.8 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Nb | % | Niobium |
| Mo | % | Molybdenum |