XH75MT
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % | Ti, % | Ni, % | Mo, % |
|---|---|---|---|---|---|
| 0.7–11 | 13–16 | 1–2.3 | 66.7–83.3 | 2–4 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Mo | % | Molybdenum |