Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Pb, % |
P, % |
C, % |
S, % |
| TU 14-1-2918-80 |
< 1 |
< 0.6 |
< 0.4 |
19–22 |
2.65–2.95 |
71.947–77.61 |
0.7–1 |
< 0.001 |
< 0.015 |
0.04–0.08 |
< 0.007 |