IMV2 (MA21)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Magnesium |
Wrought Magnesium Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Na, % |
Li, % |
Cd, % |
Ce, % |
K, % |
OE, % |
| GOST 14957-76 |
< 0.03 |
< 0.1 |
77.965–83.2 |
< 0.1 |
< 0.04 |
1–2 |
< 0.005 |
4.3–5.3 |
< 0.005 |
7.5–9 |
4–5 |
< 0.15 |
< 0.005 |
< 0.3 |