ISO 5832-4
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Cobalt |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | C, % | Mo, % |
|---|---|---|---|---|---|---|---|---|
| GOST R ISO 5832-4-2011 | < 1 | < 1 | < 1 | 58.965–69 | 26.5–30 | < 1 | < 0.035 | 4.5–7 |
Information on suppliers
Analogues
| Germany |
|---|
| ISO 5832-4 DIN ISO 5832-4 |
Standards
| Standard | Description |
|---|---|
| GOST R ISO 5832-4-2011 | GOST R ISO 5832-4-2011 |