Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
| TU 14-1-3917-85 |
0.9–1.5 |
0.1–0.5 |
0.5–1 |
0.25–1 |
27–30 |
61.787–69.15 |
2–4 |
< 0.008 |
0.1–0.2 |
< 0.005 |