K63 (63)
for the manufacture of crane rails
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Steels for special purposes | Steel for rail transport |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | As, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST Р 51685-2000 | 96.832–98.72 | 0.15–0.35 | 0.6–1 | < 0.3 | < 0.3 | < 0.3 | < 0.08 | < 0.05 | 0.53–0.73 | < 0.05 | < 0.008 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Alloy | GOST 4121 - 96 | 731 | 372 | 6 |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Alloy | GOST 4121 - 96 | 212 |
Standards
| Standard | Description |
|---|---|
| GOST Р 51685-2000 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |