Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
P, % |
C, % |
S, % |
| GOST 1215-79 |
94.44–96 |
1–1.6 |
0.4–0.6 |
< 0.08 |
< 0.18 |
2.6–2.9 |
< 0.2 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
| 20 |
1.55 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Casting |
GOST 1215-79 |
|
|
|
294 |
6 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
GOST 1215-79 |
|
100–163 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |