Kd0000
High purity cadmium is used for the production of chemically pure reagents and for scientific purposes.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Metals and alloys |
Cadmium |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Pb, % |
Cd, % |
Ag, % |
In, % |
Tl, % |
Hg, % |
Примеси, % |
| GOST 22860-93 |
< 5.0E-6 |
< 2.0E-6 |
< 1.0E-6 |
< 1.0E-5 |
< 2.0E-6 |
< 1.0E-5 |
> 99.9999 |
< 1.0E-6 |
< 2.0E-6 |
< 1.0E-5 |
< 8.0E-5 |
< 0.0001 |
Note: By agreement: Hg <0.01
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8650 |
Casting and technological parameters
| melting point, °C |
Boiling temperature, °C |
| 321 |
770 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Pb |
% |
Lead |
| Cd |
% |
Cadmium |
| Ag |
% |
Silver |
| In |
% |
Indium |
| Tl |
% |
Thallium |
| Hg |
% |
Mercury |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Boiling temperature |
°C |
The boiling point, boiling point is the temperature at which the liquid under constant pressure boils. |