Kd0A
For the manufacture of ingots, plates and rods used in various industries.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Metals and alloys |
Cadmium |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
As, % |
Cd, % |
Tl, % |
Примеси, % |
| GOST 1467-93 |
< 0.0003 |
< 0.001 |
< 0.004 |
< 0.001 |
< 0.001 |
< 0.001 |
< 0.008 |
< 0.001 |
> 99.98 |
< 0.002 |
< 0.02 |
Note: As + Sb + Sn <0.003
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
8650 |
Casting and technological parameters
| melting point, °C |
Boiling temperature, °C |
| 321 |
770 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| Cd |
% |
Cadmium |
| Tl |
% |
Thallium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Boiling temperature |
°C |
The boiling point, boiling point is the temperature at which the liquid under constant pressure boils. |