Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
O, % |
N, % |
H, % |
Примеси, % |
|
50.341–54.5 |
< 0.28 |
< 0.4 |
17–18.5 |
< 0.1 |
< 0.1 |
< 0.2 |
28.5–29.7 |
< 0.2 |
< 0.015 |
< 0.03 |
< 0.015 |
< 0.008 |
< 0.01 |
< 0.001 |
< 0.1 |
Information on suppliers
Analogues
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| O |
% |
Oxygen |
| N |
% |
Nitrogen |
| H |
% |
Hydrogen |