KS741
For ingots produced from primary metals, scrap and waste of non-ferrous metals and alloys, and intended for the production of engine pistons.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|
| GOST 30620-98 | < 0.5 | 19–22 | 0.7–1.2 | 0.6–1 | 1.8–2.4 | 1.1–1.7 | 71.2–76.8 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 30620-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |