KT-2
For the production of cold drawn wire, used for the manufacture of springs are wound in a cold state and not be quenched.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Spring-spring structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 9389-75 | 98.08–98.53 | 0.17–0.37 | 0.2–0.4 | < 0.05 | < 0.1 | < 0.05 | < 0.02 | 0.86–0.91 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 9389-75 | GOST 9389 - 75 |