KTN-20

It has high hardness, but lower bending strength. It has a low clingability with steels. Works on steels with virtually no buildup. It is used for (finishing and semi-finishing turning and milling of low-alloyed, carbon steels, cast iron and non-ferrous alloys). Wear resistance is 1.2 — 1.5 times higher than that of alloys of the TK group. Disadvantage — poorly solder and sharpening

For finishing and semi-finishing turning and milling of low-alloyed, carbon steels, cast iron and non-ferrous alloys.

Classification

Country Section Category
CIS, Russia, Ukraine Refractory metals, carbide Hard Sintered Tungsten Free Alloys

Information on suppliers

Physical characteristics

Temperature, °C $$\rho$$, $$\frac{kg}{m^3}$$
20 6.17

Standards

Standard Description
GOST 26530-85

Description of physical characteristics

Parameter Units of measurement Description
$$\rho$$ $$\frac{kg}{m^3}$$ The density of the material