KTN-30
It has high hardness, but lower bending strength. It has a low clingability with steels. Works on steels with virtually no buildup. It is used for (finishing and semi-finishing turning and milling of low-alloyed, carbon steels, cast iron and non-ferrous alloys). Wear resistance is 1.2 — 1.5 times higher than that of alloys of the T. K.
For finishing and semi-finishing turning and milling of low-alloyed, carbon steels, cast iron and non-ferrous alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard Sintered Tungsten Free Alloys |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 6.4 |
Standards
| Standard | Description |
|---|---|
| GOST 26530-85 |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |