L114
Production of ingots and cast rods intended for further refining in the production of shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90127 - 85 | < 1.5 | < 0.4 | < 0.04 | < 0.4 | 10–12 | 10–12 | 2.2–3 | 55.525–66.15 | 5.5–6.8 | < 0.01 | < 0.015 | 0.15–0.3 | < 0.01 | 3–4 | 3–4 |
Information on suppliers
Long-term strength
| Standard | Treatment | Температура испытаний, ° С | Постоянно приложенное напряжение, МПа | Время до разрушения в часах, ч |
|---|---|---|---|---|
| OST 1-90127 - 85 | Heating to a temperature of 1200 ± 10 ° С, holding 4 - 4.5 hours, air cooling | 975 | 200 | 40 |
Standards
| Standard | Description |
|---|---|
| OST 1-90127 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |