LAZhMTS66-6-3-2 (LAZhMts)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Mg, % | Cu, % | Zn, % | Sb, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|---|---|
| 2–4 | < 1 | 1.5–2.5 | 64–68 | < 16.4 | < 0.1 | 6–7 | < 1 |