LE-1
Active catalysts for the production in an industrial synthesis, as a degasser, modifier, and as an additive for metal alloys to reduce color their density, increase corrosion resistance and improve the mechanical characteristics of the alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Lithium |
Chemical composition
| Standard | Fe, % | Mg, % | Ca, % | Mn, % | Al, % | Na, % | Li, % | N, % | K, % | oxide Si, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 8774-75 | < 0.005 | < 0.02 | < 0.03 | < 0.001 | < 0.003 | < 0.04 | 99.836–99.985 | < 0.05 | > 0.005 | > 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 8774-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| K | % | Potassium |
| oxide Si | % | Silicon oxide |
| Mg | % | Magnesium |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Al | % | Aluminium |
| Na | % | Sodium |
| Li | % | Li |
| N | % | Nitrogen |