PLW (LZHS58-1-1)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
P, % |
Примеси, % |
| GOST 2171-90 |
0.7–1.3 |
< 0.003 |
56–58 |
38.367–42.6 |
< 0.5 |
< 0.01 |
0.7–1.3 |
< 0.02 |
< 0.5 |