LK
The feedstock material for LTS16K4 brass. Complex configuration instrument parts and fittings for use in sea water; gear; details of friction units
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Brass (copper-zinc alloy) | Foundry brass ingots |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | P, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1020-97 | < 0.6 | 2.8–4.5 | < 0.3 | 76–81 | 12–21.2 | < 0.2 | < 0.1 | < 0.1 | < 0.5 | < 0.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1020-97 | Cast brass ingots. Grades. |
| GOST 2171-90 | GOST 2171-90 |
| DSTU 3473-96 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| P | % | Phosphorus |