LK4
Production of ingots and cast rods intended for further refining in the production of shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90127 - 85 | < 1.5 | < 0.5 | < 0.6 | 59.35–67.35 | 25–28 | 3–3.75 | < 0.025 | 0.15–0.25 | < 0.025 | 4.5–5.5 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1-90127 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |