LK62-0.5
Complex alloyed brass
For the manufacture of wire rods for gas welding and brass welding of carbon steel
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Brass (copper-zinc alloy) | Brass, pressure treated |
Chemical composition
| Standard | Fe, % | Si, % | Bi, % | Cu, % | Zn, % | Sb, % | Pb, % |
|---|---|---|---|---|---|---|---|
| GOST 15527-2004 | < 0.15 | 0.3–0.7 | < 0.002 | 60.5–63.5 | 35.07–38.7 | < 0.005 | < 0.08 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 8400 |
Standards
| Standard | Description |
|---|---|
| GOST 15527-2004 |