LK75-0.5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Si, % | Sn, % | Cu, % | Zn, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|
| TU 48-0808-17-94 | < 0.5 | < 0.05 | 71–78 | 20–29 | < 0.03 | < 1.42 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-0808-17-94 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Pb | % | Lead |