LMtsSKA58-2-2-1-1 (LMtsSKA)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Bi, % |
Mn, % |
Cu, % |
Zn, % |
Sb, % |
Al, % |
Pb, % |
P, % |
Примеси, % |
| TU 48-0814-44-91 |
< 0.6 |
0.5–1.2 |
< 0.002 |
1.75–2.5 |
57–60 |
31.183–38.65 |
< 0.005 |
0.6–1.2 |
1.5–2.2 |
< 0.01 |
< 1.1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |