LOS
The feedstock material for LTS25S2 brass. Connections hydraulic cars
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Brass (copper-zinc alloy) | Foundry brass ingots |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1020-97 | < 0.7 | < 0.5 | 0.5–1.5 | < 0.5 | 53.9–79.5 | 19–38.5 | < 1 | < 0.1 | < 0.3 | 1–3 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| G-Ms65 | 60-40 |
| 2.0291 |
Standards
| Standard | Description |
|---|---|
| GOST 1020-97 | Cast brass ingots. Grades. |
| GOST 2171-90 | GOST 2171-90 |
| DSTU 3473-96 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |