LS60-2
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
Примеси, % |
| GOST 15527-70 |
< 0.2 |
< 0.2 |
59–62 |
33.98–40 |
< 0.5 |
< 0.02 |
1–2.5 |
< 0.6 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |